20-05-2014, 09:55 PM
The 1:1 ratio is mainly used with cellulose paint and solvent base coats.
But if you use 2k stuff read the tech sheet as some companies use different ratios i.e 4:1 for primers and lacquers etc.
As for pressure the average HVLP gun pressure is about 30/40psi when trigger fully depressed.
But if you use 2k stuff read the tech sheet as some companies use different ratios i.e 4:1 for primers and lacquers etc.
As for pressure the average HVLP gun pressure is about 30/40psi when trigger fully depressed.